Maxipur 25% component A (large tin) and component B (small tin)

Maxipur

2-component solvent-based PU varnish

Solvent-based 2-component PU varnish for very heavy wear, in three versions from thick to thin.

Made to order

866 kr incl. VAT

Call 400 08 038

A company? Log in to Zenzorama Proff and see your price excl. VAT.

Mixing ratio
4 L varnish + 1 L hardener (25 %), + 2 L (50 %) or + 4 L (100 %)
Consumption
8 to 9 m² per litre
Pot life at 20 °C
4 hours (50 % and 100 %), 3 hours (25 %); workable for approx. 2 hours
Dust-dry
4 hours
Next coat
after 4 hours, within 3 days at the latest
Water on the surface
after 48 hours at the earliest
Cleaning agents and covering
after 2 weeks at the earliest
Working conditions
substrate above 10 °C and at least 3 °C above the dew point
Sheen level
matt, satin and gloss

About Maxipur

Maxipur is a solvent-based 2-component polyurethane varnish that does not yellow. The percentage tells you how much hardener is mixed into the varnish: 25 % is 1 litre of hardener to 4 litres of varnish, 100 % is equal parts. The lower the percentage, the thicker the varnish and the thicker the film. The higher the percentage, the thinner the varnish and the better it penetrates.

Choose when
When the surface gets very heavy wear and you choose a solvent-based varnish.
Place in the build-up
After Hydroprimer on finished microcement, when the colour is to be preserved. The number of coats depends on how absorbent the surface is.

Variants

VariantCemher's nameDescription
Maxipur 25 %, thick and fillingMaxipur 25%4 L varnish and 1 L hardener give the thickest varnish, with the thickest film and the most body.
Maxipur 50 %, mediumMaxipur 50%4 L varnish and 2 L hardener give a medium-thick varnish that, according to Cemher, penetrates better than 25 %.
Maxipur 100 %, thin and penetratingMaxipur 100%Equal parts varnish and hardener give the thinnest varnish, which penetrates best.

Good to know

  • Solvent-based and for professional use. Ensure good ventilation and wear a mask with a filter for organic solvents.
  • According to Cemher, Hydroprimer can be omitted on microcement that is watertight in the material, but it is needed when the colour is to be preserved.